Guys I have been trying the dip method with some moisture cured urethane and 5 out of 10 baits will have wrinkled paint about 30 seconds after dipping. I have tried everything I know to do. I have been told that the paint may have not been heat set good enough. I tried heat setting the paint for twice as long as I normally do.......same result. My painting process is:
1. Sand the bait with 400 grit
2. clean the bait with wax and grease remover
3. Auto air sealer for the base
4. Createx or auto air paints with heat setting after every coat
5. heat set again for a good bit after the painting process has been completed
6. let the bait set at least 24 hours after I finish painting
I am just not sure what I am doing wrong and why I can't get this stuff to work on 5 or 6 baits in a row, then the next 3 wrinkle
I do the dipping in a spare room in the house and I usually keep the temperture around 72-74 degrees.......so help me out guys, please!