kahawai Posted November 24, 2008 Report Share Posted November 24, 2008 (edited) hi all, i have been experimenting with foiled and painted finish on my latest lure. i am fairly new to this combination. i normally do fully painted or photofinish on foil. But i wanted maximum flash on this lure so decided to use foil with translucent and opaque paints. here's a pic of it. it's a mini sized slow sinking left-right jerkbait/glider. tight lines peter if you're interested more pics here- Image hosting, free photo sharing & video sharing at Photobucket Edited November 24, 2008 by kahawai Quote Link to comment Share on other sites More sharing options...
BobP Posted November 24, 2008 Report Share Posted November 24, 2008 Kahawai, very nice bait. You Photobucket pics show some superb finishes! Quote Link to comment Share on other sites More sharing options...
Husky Posted November 24, 2008 Report Share Posted November 24, 2008 It's good to see you back! I've always been a big fan of your work!! [quote name='kahawai;1 11107]hi all' date=' i have been experimenting with foiled and painted finish on my latest lure. i am fairly new to this combination. i normally do fully painted or photofinish on foil. But i wanted maximum flash on this lure so decided to use foil with translucent and opaque paints. here's a pic of it. it's a mini sized slow sinking left-right jerkbait/glider. [img']http://i31.photobucket.com/albums/c376/big_kahawai/IMG_3112.jpg[/img] tight lines peter if you're interested more pics here- Image hosting, free photo sharing & video sharing at Photobucket Quote Link to comment Share on other sites More sharing options...
hazmail Posted November 24, 2008 Report Share Posted November 24, 2008 Pete - nice work with the foil, and I had a look at Photobucket, you obviously have put in an amazing number of hours on them, for some great colour combos. I recently fished a few of my foiled (mylar) lures, and found the finish coat was chipping off in slabs - we need to come up with a primer to bind to the foil and for the topcoat to stick to, any ideas here? These lures were coated with D2T, which may be the problem . pete Quote Link to comment Share on other sites More sharing options...
jamie Posted November 24, 2008 Report Share Posted November 24, 2008 Pete - nice work with the foil, and I had a look at Photobucket, you obviously have put in an amazing number of hours on them, for some great colour combos.I recently fished a few of my foiled (mylar) lures, and found the finish coat was chipping off in slabs - we need to come up with a primer to bind to the foil and for the topcoat to stick to, any ideas here? These lures were coated with D2T, which may be the problem . pete Pete is the foil lifting or are you having problems with the top coat itself sticking to the foil? Quote Link to comment Share on other sites More sharing options...
LooksLikeSinbad Posted November 26, 2008 Report Share Posted November 26, 2008 That looks awesome! Quote Link to comment Share on other sites More sharing options...
CA Delta Posted November 26, 2008 Report Share Posted November 26, 2008 Wow your lures look great. Keep up the good work. Man you guys make painting look so easy. I'm just starting out, maybe I could become someones apprentice. Quote Link to comment Share on other sites More sharing options...
hazmail Posted November 26, 2008 Report Share Posted November 26, 2008 Jamie - Just the D2T is coming off, the foil is as good as new, just needs a 'Primer' for the D2T to stick to.pete Quote Link to comment Share on other sites More sharing options...
kahawai Posted November 26, 2008 Author Report Share Posted November 26, 2008 thanks all! pete,d2t coming off in chunks? i have not had that happen before. on the couple of fully foiled baits i have done, i spray a thin layer of clear acrylic to seal the text and fin colours in before applying the top coat. now i wonder if that helps to hold the d2t. also the 2 lures have scale texture on the foil, so that may help the d2t hold too. husky, its good to be back! work doesn't allow me to spend as much time on the lures as i'd like nowadays. I learnt all my stuff from here! so you have to take some of the credit. tight lines. Quote Link to comment Share on other sites More sharing options...
mark poulson Posted November 26, 2008 Report Share Posted November 26, 2008 (edited) Jamie - Just the D2T is coming off, the foil is as good as new, just needs a 'Primer' for the D2T to stick to.pete Just a guess. I had the same problem with my wood baits when I used D2T for a top coat. When I switched, first to Etex Lite, and now to Nu Lustre 55 with UV inhibiters, the problem went away. Now, if I have an encounter with a jumping rock, the kind that move into the line of my cast, I get a dent, not a delamination. To start with, foil is slick. I think you probably need a clear "primer" to get some bond to the foil. Like a matte clear. Maybe pastel fixative. Almost any rattle can clear has better adhesion than water based paints. Then top coat with a decopage-type epoxy, like Etex or Nu Lustre. Those epoxies are more flexible than D2T, which is a glue and very rigid. Kahawai, I saw you photobucket stuff. Great looking lures, and amazing paint jobs! Edited November 26, 2008 by mark poulson Quote Link to comment Share on other sites More sharing options...
jamie Posted November 27, 2008 Report Share Posted November 27, 2008 Jamie - Just the D2T is coming off, the foil is as good as new, just needs a 'Primer' for the D2T to stick to.pete Pete im an etex man myself and I dont have any experience with d2t. I will have to say that 90% of all my baits are foiled and I never had that to happen to me.I have tried crystal sheen before and it didnt work well with the foil, alot of cracking. It could be that d2t has no flexability to it its and its hard as a rock, and it chips off in big chunks.It could be a temp issue, some foil baits in direct sun or in a hot tackle box all day with certain clears has major issues. Give etex a shot and see if the same problem happens and let me know Im curious to see if that would make the difference. Quote Link to comment Share on other sites More sharing options...
hazmail Posted November 27, 2008 Report Share Posted November 27, 2008 Thanks guys, for all the cures, I usually do prime the paint with Pastel Fixative or clear schelac, but for some reason did not with the Mylar - as you are all saying, this would be a major reason for the delamination. I am still using D2T, as I have a few tubes to get rid of, and then will probably go to a version of moisture cure Poly or Etex. Thanks again . pete Quote Link to comment Share on other sites More sharing options...
gotcha man Posted December 6, 2008 Report Share Posted December 6, 2008 Where do I get the foil and fins to try on my wooden muskie lures? Terry Quote Link to comment Share on other sites More sharing options...
borderbasser Posted December 6, 2008 Report Share Posted December 6, 2008 Has anyone tried Dicknite's? I have been considering doing a foil job, but have been having a hard time bringing my self to try it since all I make are multiple jointed swimbaits TJ Quote Link to comment Share on other sites More sharing options...
rofish Posted December 6, 2008 Report Share Posted December 6, 2008 Hazmail, I remember that a wise man said once that he tries the epoxy first, before applying it on baits, or something like that. He would put some on different materials, to see how how strong the epoxy was. Why don't you put some epoxy on mylar and on different types of foil, to see how strong is the bond between epoxy and mylar? I might guess that epoxy does not bond too well to mylar. But there are also some other reasons why I do not like to use mylar instead of foil. Quote Link to comment Share on other sites More sharing options...
b1gf1sh1 Posted December 6, 2008 Report Share Posted December 6, 2008 on the d2t issue. yes to UV resistant clear. also, have you ever tried adding two drops of 99% isopropyl and 1 drop of ammonia to your d2t per 4 drams? i really don''t have a-lot of experience with the d2t but this just may help with the flex issue. and extend the cure time a bit helping it to flow out better. it works on other fast drying epoxies and i see no reason it won't. it will reduce the tensile but it will enhance the impact resistance and elongation. two of the more important features in a lure coating. most will know this but for those who don't... in general, the faster an epoxy cures the more brittle it will be. Quote Link to comment Share on other sites More sharing options...
kahawai Posted December 6, 2008 Author Report Share Posted December 6, 2008 Where do I get the foil and fins to try on my wooden muskie lures?Terry i use adhesive insulation foil from the hardware shop. the fins on my lures are drawn/etched into the foil and then painted. i haven't tried those wonderful looking micro fibettes fins yet, but am keen to do so at some time... --------- see my gingermojo lures Image hosting, free photo sharing & video sharing at Photobucket Quote Link to comment Share on other sites More sharing options...
jflures Posted December 6, 2008 Report Share Posted December 6, 2008 on the d2t issue. yes to UV resistant clear. also, have you ever tried adding two drops of 99% isopropyl and 1 drop of ammonia to your d2t per 4 drams? i really don''t have a-lot of experience with the d2t but this just may help with the flex issue. and extend the cure time a bit helping it to flow out better. it works on other fast drying epoxies and i see no reason it won't. it will reduce the tensile but it will enhance the impact resistance and elongation. two of the more important features in a lure coating.most will know this but for those who don't... in general, the faster an epoxy cures the more brittle it will be. This is a good point about the dry time! I "thin" my D2T with acetone. I pour out about a quater size circle of D2T add 2 drops of acetone mix well and apply. It takes about 4 hours for it to harden enough to touch. I have had no problems with chipping of any kind. Quote Link to comment Share on other sites More sharing options...
Lure--Prof Posted December 6, 2008 Report Share Posted December 6, 2008 Has anyone tried Dicknite's? I have been considering doing a foil job, but have been having a hard time bringing my self to try it since all I make are multiple jointed swimbaits TJ After painting, I normally coat my foil lures with either Etex, before my usual 3 coats of Dicknite's, because DN doesn't want to stick to foil. Lightly sand or scuff the E-tex and give it an alcohol wipe before applying the Dicknite's on top of the E-tex, and avoid contaminating the lure with fingerprints before the DN goes on. Dean Quote Link to comment Share on other sites More sharing options...
b1gf1sh1 Posted December 7, 2008 Report Share Posted December 7, 2008 jflures acetone works but because of the evap rate it can cause blushing. also my information indicates that it will be more apt to soak in water from larger pores created with acetone and swell. i can't say it's going to be a huge problem because i never ''tested'' the amount of swelling. with the mix i proposed it's much less, that's all i know. almost any aliphatic solvent without a high water content will work but 99% isopropyl is best with the ammonia blend. too harsh a solvent and it burns it away. good luck. Quote Link to comment Share on other sites More sharing options...