Jump to content
borderbasser

OOMOO RTV and Lead

Recommended Posts

Does anyone have any experiece using OOMOO from Smooth-on for pouring lead? I know that the platinum cure RTV is a better choice, but I already have some of the tin cure OOMOO. I am needing to pour some swimbait harnesses and won't be making a lot of them anyway. Will this stuff hold up to the heat of say about 20 harnesses? Thanks guys.

TJ

Link to comment
Share on other sites

Does anyone have any experiece using OOMOO from Smooth-on for pouring lead? I know that the platinum cure RTV is a better choice, but I already have some of the tin cure OOMOO. I am needing to pour some swimbait harnesses and won't be making a lot of them anyway. Will this stuff hold up to the heat of say about 20 harnesses? Thanks guys.

TJ

Hi TJ,

I think you will be OK. I used it to pour some thick & heavy dolphin/dorado jigheads & got about half a dozen pours before the oomoo mold distorted.

Give some time between pours to let the silicone cool down.

omoo isn't ideal, but again, for short runs you should be ok.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Loading...


×
×
  • Create New...
Top