tightliner Posted February 5, 2010 Report Share Posted February 5, 2010 Hi Guys. I've painted some of my wiggle warts with lacquer paint. First sanded, primed with super hide laquer,let dry well, painted the pattern and let dry well. I then dipped in Dn, let it stand a week. the body of the lure is hard as a rock and very shiney. The problem is with the edge of the bill. You can simply scratch it off with your finger nail with not much pressure. I was wondering if an adhesion promotor would help with the "edge" issue. And if so what brand and what stage in the painting process. I really like Dn and this is really the only issue I've had , it could very well be my technique. If anyone would be willing to advise, please do. Thanks alot, Ed. Quote Link to comment Share on other sites More sharing options...