Some flakes will curl if the plastic is heated beyond 350 degrees or reheated; some don't. I've been trying to find a source of flakes (similar to LC) that resist higher temps. The only solution I've found is to add flakes when the plastic cools a little, but to cool to pour. The shape will stay the same, at least for the first pours.