Grenouille Posted July 31, 2011 Report Share Posted July 31, 2011 Hi guys, i 'd got a recent problem with my hand injectors, specially visible when pouring translucid plastic. a kind of black deposit was visible in lures after injecting. i suspect the problem comes from the O ring and not the aluminium itself.. my hand 'jectors comes from Bears and never had this problem before since near 2 years... one time, i wanted to clean my injectors with Acteone and for sure the problem comes from that(noob) mistake? if someone could illuminate my lantern, as we say in france, it would be great appreciated..thanx Quote Link to comment Share on other sites More sharing options...
SHK Posted July 31, 2011 Report Share Posted July 31, 2011 very well could be the issue, get ahold of Bear and get a replacement set of o-rings. i usually use a dab of softener or worm oil to clean and lubricate Quote Link to comment Share on other sites More sharing options...
jigtwins Posted July 31, 2011 Report Share Posted July 31, 2011 Hi guys, i 'd got a recent problem with my hand injectors, specially visible when pouring translucid plastic. a kind of black deposit was visible in lures after injecting. i suspect the problem comes from the O ring and not the aluminium itself.. my hand 'jectors comes from Bears and never had this problem before since near 2 years... one time, i wanted to clean my injectors with Acteone and for sure the problem comes from that(noob) mistake? if someone could illuminate my lantern, as we say in france, it would be great appreciated..thanx I use viton high temp seals in my injectors.Had the same problem too. the black orings were not holding up to the temps of the plastic, causing them to bleed into my baits. Viton is good to around 450F. Just my experience with this issue. Quote Link to comment Share on other sites More sharing options...
powerworm Posted July 31, 2011 Report Share Posted July 31, 2011 dont use the replacement ones from like a home improvement store order the correct oring from mcmaster or granger or you might have something overseas to avoid all the paperwork Quote Link to comment Share on other sites More sharing options...
Grenouille Posted August 5, 2011 Author Report Share Posted August 5, 2011 (edited) thanx guys for answer, do y have a link for "viton" and a link for the good size of O ring on mcmaster or granger store? i tried to find but was lost on their website... Edited August 5, 2011 by Grenouille Quote Link to comment Share on other sites More sharing options...
powerworm Posted August 5, 2011 Report Share Posted August 5, 2011 search under high-temp is what i did when i ordered some last year then check what its made of it will say in the description and use only viton orings. Quote Link to comment Share on other sites More sharing options...
Grenouille Posted August 9, 2011 Author Report Share Posted August 9, 2011 thanx a lot, Powerworm, i found it and ordered, hope it will solve the problem...translucid colors are a must here in france during summer Quote Link to comment Share on other sites More sharing options...