Pikestalker Posted May 11, 2012 Report Share Posted May 11, 2012 I have been poring for a while now, with remelted soft baits. It has been working pretty good, but i bought some LC plastisol and i just can´t get the two layers of plastic to bond in the mold. i pour pretty much one color after the other. Also the baits come out feeling very greasy, anyone have any ideas how to work this problem out? Maybe just buy another brand? Quote Link to comment Share on other sites More sharing options...
SHK Posted May 11, 2012 Report Share Posted May 11, 2012 what temps are you measuring? Quote Link to comment Share on other sites More sharing options...
Bass-Boys Posted May 11, 2012 Report Share Posted May 11, 2012 make sure you shake up the plastic well.. it settles a lot.. you have to have 100% of the settlings mixed up. not being mixed well will give you greasy or sticky baits,, and as SHK asked above,, the temp is very important on a laminate, you need it to be hot !!! apx. 340 - 350 deg. but, do not over heat it and burn it Quote Link to comment Share on other sites More sharing options...
Pikestalker Posted May 11, 2012 Author Report Share Posted May 11, 2012 Thanks for your advice guys, didn´t realize temprature was that important. Quote Link to comment Share on other sites More sharing options...
Bass-Boys Posted May 12, 2012 Report Share Posted May 12, 2012 to get 2 colors to adhere to each other it must be hot enough to melt together not so hot with a non laminate. Quote Link to comment Share on other sites More sharing options...