bluetickhound Posted July 4, 2013 Report Share Posted July 4, 2013 Got some BT holographic glitter the other day and really like the look of it.... My problem is that when I heat the plastic enough to pour correctly ( and I am hand pouring these worms, not injecting) the glitter shrivels up and/or "taco's" on me. Should I add the glitter while the plastic is still cold or just add the heat more slowly or what? I know now that (unlike almost every other glitter I use) you can't just heat up the plastic and toss in the glitter... This stuff actually made popping noises like Rice Krispies when I added it today... I need to know the balance between getting the plastic up to the correct temp to pour without ruining the glitter in the process... Quote Link to comment Share on other sites More sharing options...
Frank Posted July 5, 2013 Report Share Posted July 5, 2013 When you say hot enough do you know what temp it is? I use that stuff all the time but no folding issue. Now red and blue yes even at lower temps it does that for me. Quote Link to comment Share on other sites More sharing options...