Hunter04 Posted August 13, 2020 Report Share Posted August 13, 2020 i have recently gotten into making senkos. i have been turning my salt into a powder in the coffee grinder but when i inject the mold there are clumps of salt in the worms. what should i do? Quote Link to comment Share on other sites More sharing options...
wallyc14 Posted August 16, 2020 Report Share Posted August 16, 2020 My personal take on it is easy. I mix my salt with my plastic before I heat. Since doing this 7 years ago no more clumps. I’m sure someone will have a different answer but this works for me if I grind salt. Now I just buy worm salt way easier but I still mix the same way . 1 Quote Link to comment Share on other sites More sharing options...
Bass-Boys Posted August 16, 2020 Report Share Posted August 16, 2020 just more mixing before you fill the injector,, The salt will settle to the bottom of your pyrex so mix well , then fill injector ASAP . 1 Quote Link to comment Share on other sites More sharing options...
The Rook Posted August 17, 2020 Report Share Posted August 17, 2020 (edited) Fine Grit glass bead media. Works much better than salt, doesn't clump or cloud the color of the plastic. It also adds durability to the bait. It can be a little rough on the injector however. Just throwing another option out there. Edited August 17, 2020 by The Rook 1 Quote Link to comment Share on other sites More sharing options...
wallyc14 Posted August 17, 2020 Report Share Posted August 17, 2020 Yep! Works good but it’s hell on the injector. If you go that route I would highly recommend only using one injector for it. I have a 4 oz injector from bears is the one I use and it’s scared up pretty good 1 Quote Link to comment Share on other sites More sharing options...
mark poulson Posted August 20, 2020 Report Share Posted August 20, 2020 Be sure you get virgin blasting beads, so the glass isn't broken. Quote Link to comment Share on other sites More sharing options...
Bassmaster Rick Posted August 23, 2020 Report Share Posted August 23, 2020 On 8/17/2020 at 3:00 PM, wallyc14 said: Yep! Works good but it’s hell on the injector. If you go that route I would highly recommend only using one injector for it. I have a 4 oz injector from bears is the one I use and it’s scared up pretty good Can you reheat your plastic when using GBM? I've heard it's not recommended. Quote Link to comment Share on other sites More sharing options...
wallyc14 Posted August 23, 2020 Report Share Posted August 23, 2020 Oh yeah! Never had problems there. 2 Quote Link to comment Share on other sites More sharing options...
Just_Wil Posted September 5, 2020 Report Share Posted September 5, 2020 Heard of this fine glass media several times now....but does anyone have a secret source with a ready supply? Quote Link to comment Share on other sites More sharing options...
wallyc14 Posted September 5, 2020 Report Share Posted September 5, 2020 Sure! Amazon it’s where I get mine 1 Quote Link to comment Share on other sites More sharing options...
mark poulson Posted September 6, 2020 Report Share Posted September 6, 2020 22 hours ago, Just_Wil said: Heard of this fine glass media several times now....but does anyone have a secret source with a ready supply? https://www.ebay.com/itm/8-LBS-Glass-Bead-Medium-Grit-MIL-SPEC-8-70-100-grit-Sand-Blasting-Abrasive-/111672165459?hash=item1a002e0453:g:VocAAOxydgZTKU6c Quote Link to comment Share on other sites More sharing options...